Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Shinkong Synthetic Fibers Corp
Trade Name Shinite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 127 MPa
18500 psi
ASTM D638
Elongation at Break 3.6 %
3.6 %
ASTM D638
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Flexural Modulus 9.41 GPa
1370 ksi
ASTM D790
Izod Impact, Notched 0.883 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.65 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 4.0
4.0
ASTM D150
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149