SABIC Innovative Plastics LNP Verton MV00ASUV_WH9D703 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Verton MV00ASUV_WH9D703 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Preliminary data for 50% Long fiber single color pellet filled PPThis data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 136 MPa
19700 psi
5 mm/min; ISO 527
Tensile Strength, Yield 136 MPa
19700 psi
5 mm/min; ISO 527
Elongation at Break 1.9 %
1.9 %
5 mm/min; ISO 527
Elongation at Yield 1.9 %
1.9 %
5 mm/min; ISO 527
Tensile Modulus 8.83 GPa
1280 ksi
1 mm/min; ISO 527
Flexural Strength 199 MPa
28900 psi
2 mm/min; ISO 178
Flexural Modulus 9.43 GPa
1370 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²

@Temperature -40.0 °C
10.5 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
22.0 kJ/m²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 53.0 kJ/m²

@Temperature 23.0 °C
25.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
11.0 J

@Temperature 23.0 °C
8.11 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af