Solvay Engineered Polymers SEQUEL® 1440LS TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1440LS TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processability, and good paint adhesion. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
as molded; ISO 294
0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
after bake; ISO 294
Melt Flow 21 g/10 min
21 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.17 GPa
170 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 18.0 J
13.3 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228