Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.903 GPa | 131 ksi | ASTM D790 |
Formosa Plastics Formolene® LH5320 Injection Molding HDPE
(discontinued **) CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5320 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | ASTM D790 |
Formosa Plastics Formolene® LH5326 Injection Molding HDPE
(discontinued **) CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5326 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ CB272 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB272 high melt flow, 900 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of rigidity and dime.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | Secant; ISO 178 |
ExxonMobil Exxtral™ BNT 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior painted parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific, Europe, South A.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | Secant; ISO 178 |
ExxonMobil Exxtral™ BNT 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific,.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | ASTM D790 |
Entec Hypel® PEHD20/.953 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | ISO 178 |
ExxonMobil PP8013L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu.. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | ASTM D790 |
Amco PRIMATOP HDPE 175953 Injection Molding Polyethylene HDPE 175953 features easy flow, toughness, and high surface gloss. Applications include caps, thin wall parts, and toys.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Flexural Modulus | 0.903 GPa | 131 ksi | ISO 178 |
LyondellBasell Hifax™ ETA3163/1 Thermoplastic Polyolefin Elastomer Description: Hifax™ ETA3163/1 medium melt flow, 900 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness and low temper.. |