Amco PRIMATOP HDPE 175953 Injection Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP HDPE 175953 Injection Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HDPE 175953 features easy flow, toughness, and high surface gloss. Applications include caps, thin wall parts, and toys.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Melt Index of Compound 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D638
Flexural Modulus 0.903 GPa
131 ksi
ASTM D790