Material Notes:
Dry as molded. Extrusion grade. Nylene PX1719HS is a heat stabilized, high impact, nylon 6 extrusion grade resin with a low flexural modulus. PX1719HS is ideally suited for extrusion of tubing and profiles requiring outstanding toughness and flexibility. Because of its excellent flow characteristics, it may also be used for injection molding parts requiring a high Izod impact value. Optimum processing conditions should provide a melt temperature of 520 - 540ºF at the die or nozzle.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Modulus 0.660 GPa
95.7 ksi
ASTM D790
Izod Impact, Notched 8.30 J/cm
15.5 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
286 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F