Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips HiD® 9642 HDPE Sheeting Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips HiD® 9642 HDPE Sheeting Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Containment Liners, Coextruded Liner Structures, Soil Stabilization StructuresData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 2000 hour

@Temperature 50.0 °C
>= 2000 hour

@Temperature 122 °F
F<sub>50</sub>, Cond. B.; ASTM D1693
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.660 GPa
95.7 ksi
3 pt. secant. ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 121 °C
250 °F
ASTM D1525
Brittleness Temperature <= -59.0 °C
<= -74.2 °F
ASTM D746
Users viewing this material also viewed the following: