Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.981 - 9.51 GPa | 142 - 1380 ksi | Average value: 3.93 GPa Grade Count:18 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Flexural Modulus | 3.70 - 9.50 GPa | 537 - 1380 ksi | Average value: 7.89 GPa Grade Count:23 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Flexural Modulus | 8.30 - 9.50 GPa @Temperature 80.0 - 80.0 °C |
1200 - 1380 ksi @Temperature 176 - 176 °F |
Average value: 9.10 GPa Grade Count:3 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Flexural Modulus | 0.100 - 9.50 GPa | 14.5 - 1380 ksi | Average value: 2.15 GPa Grade Count:327 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |