Material Notes:
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO R1183; ASTM D792
Moisture Absorption at Equilibrium 4.5 %
4.5 %
at equilibrium at 50% RH; ASTM D3418
4.5 %
4.5 %
at equilibrium at 50% RH; ASTM D3418
Mechanical Properties Metric English Comments
Elongation at Break >= 500 %
>= 500 %
ISO R527
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178; ASTM D790
Izod Impact, Notched NB
NB
ISO 180/ASTM D256
Thermal Properties Metric English Comments
Melting Point 204 °C
399 °F
ASTM D3418
Glass Transition Temp, Tg <= -50.0 °C
<= -58.0 °F
ASTM D3418
Optical Properties Metric English Comments
Refractive Index 1.508
1.508
ISO 489
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+9 ohm-cm
2.00e+9 ohm-cm
ASTM D257
Surface Resistance 1.50e+9 ohm
1.50e+9 ohm
ASTM D257