Polymer Property : Flexural Modulus = 0.0296 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0296 GPa
4.29 ksi
ASTM D790
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc  (discontinued **)
Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc..
Flexural Modulus 0.0296 GPa
4.30 ksi
1% secant; ASTM D790
ExxonMobil Escorene® UL 7765 Adhesive Application Resin
Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural t..
Flexural Modulus 0.0296 GPa

@Temperature 23.0 °C
4.29 ksi

@Temperature 73.4 °F
ASTM D790
DuPont™ Surlyn® 9320 Zinc Ionomer
Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin ..
Flexural Modulus 0.0296 GPa
4.30 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A
Dow FLEXOMER™ DFDA-1095 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDA-1095 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization ..
Flexural Modulus 0.0296 - 0.758 GPa
4.29 - 110 ksi
Average value: 0.308 GPa Grade Count:48
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..