ExxonMobil Escorene® UL 7765 Adhesive Application Resin

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Exxon Chemical
Trade Name Escorene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® UL 7765 Adhesive Application Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends. The resin accepts high filler level and is therfore suitable for W&C applications, in particular for haolgen free, flame retardant compounds.Availability: Asia Pacific, Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsHot Melt AdhesivesIndustrial SealantsWax BlendsBonding AdhesivesWire and Cable Compounds Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ExxonMobil Method
Vinyl Acetate Content 26.2 %
26.2 %
ExxonMobil Method
Melt Flow 2.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
15s; ASTM D2240
Hardness, Shore D 23
23
15s; ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0296 GPa
4.30 ksi
1% secant; ASTM D790
Dart Drop, Total Energy 21.7 J

@Temperature 22.8 °C
16.0 ft-lb

@Temperature 73.0 °F
ASTM D3736
24.4 J

@Temperature -40.0 °C
18.0 ft-lb

@Temperature -40.0 °F
ASTM D3736
Thermal Properties Metric English Comments
Melting Point 73.9 °C
165 °F
Peak Melting Temperature; ExxonMobil Method