Dow FLEXOMER™ DFDA-1095 NT Very Low Density Polyethylene (VLDPE) Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Dow Chemical
Trade Name FLEXOMER™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow FLEXOMER™ DFDA-1095 NT Very Low Density Polyethylene (VLDPE) Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FLEXOMER™ DFDA-1095 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to enhance toughness of the structure. Information provided by Dow
Physical Properties Metric English Comments
Density 0.886 g/cc
0.0320 lb/in³
ASTM D792
Melt Index of Compound 1.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
1 sec; molded and tested in accordance with ASTM D4976; ASTM D2240
78
78
5 sec; molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 5.93 MPa
860 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 625 %
625 %
Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 0.0296 GPa
4.30 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A
Thermal Properties Metric English Comments
Melting Point 114 °C
237 °F
Dow Method (DSC)
Glass Transition Temp, Tg -52.2 °C
-62.0 °F
reported value is for pure FLEXOMER™ DFDB-1085 NT, the primary component in this blend; Dow Method