Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 4.29 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0296 GPa
4.29 ksi
ASTM D790
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc  (discontinued **)
Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc..
Flexural Modulus 0.0296 GPa

@Temperature 23.0 °C
4.29 ksi

@Temperature 73.4 °F
ASTM D790
DuPont™ Surlyn® 9320 Zinc Ionomer
Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin ..
Flexural Modulus 0.0296 - 0.758 GPa
4.29 - 110 ksi
Average value: 0.308 GPa Grade Count:48
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..