Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.500 GPa @Temperature 80.0 °C |
72.5 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 0.500 GPa @Temperature 80.0 °C |
72.5 ksi @Temperature 176 °F |
Practical Use (Water Absorption 3.5%); ASTM-D790 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 0.500 GPa @Temperature 80.0 °C |
72.5 ksi @Temperature 176 °F |
Practical Use (Water Absorption 3.0%); ASTM-D790 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 0.500 GPa @Temperature 65.0 °C |
72.5 ksi @Temperature 149 °F |
ASTM D790 |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |