Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.00 GPa @Temperature 80.0 °C |
580 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.7%); ASTM-D790 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 80.0 °C |
580 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature -40.0 °C |
580 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.5%); ASTM-D790 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 80.0 °C |
580 ksi @Temperature 176 °F |
Practical Use (Water Absorption 1.75%); ASTM-D790 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature -40.0 °C |
580 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 80.0 °C |
580 ksi @Temperature 176 °F |
Practical Use (Water Absorption 1.6%); ASTM-D790 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |