Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 700 - 1800 MPa | 102000 - 261000 psi | Average value: 1260 MPa Grade Count:20 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Tensile Creep Modulus, 1000 hours | 650 - 1800 MPa | 94300 - 261000 psi | Average value: 1460 MPa Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Tensile Creep Modulus, 1000 hours | 1300 - 1800 MPa | 189000 - 261000 psi | Average value: 1630 MPa Grade Count:8 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Creep Modulus, 1000 hours | 1200 - 1800 MPa | 174000 - 261000 psi | Average value: 1580 MPa Grade Count:10 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Creep Modulus, 1000 hours | 1000 - 1800 MPa | 145000 - 261000 psi | Average value: 1580 MPa Grade Count:4 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |