Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 1200 - 1800 MPa | 174000 - 261000 psi | Average value: 1580 MPa Grade Count:10 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa @Strain <=0.500 % |
174000 psi @Strain <=0.500 % |
ISO 899-1 |
Styrolution Luran® S 776 S UV ASA Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j.. |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa @Strain <=0.500 % |
174000 psi @Strain <=0.500 % |
ISO 899-1 |
Styrolution Luran® S KR 2859 ASA Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa @Strain <=0.500 % |
174000 psi @Strain <=0.500 % |
ISO 899-1 |
Styrolution Luran® S KR 2859 UV ASA Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa | 174000 psi | ISO 899-1 |
Covestro Makroblend® S 7916 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa | 174000 psi | |
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe) Very easy-flowing, impact-modified grade.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa | 174000 psi | elongation <0.5%, 23°C; ISO 899-1 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa | 174000 psi | ISO 899 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Tensile Creep Modulus, 1000 hours | 1200 MPa | 174000 psi | |
Arkema Group Oroglas® MI-7T Acrylic
(discontinued **) OROGLAS MI-7T is a medium impact grade combining excellent thermal resistance with good impact performance.Key features : impact resistance: up to 7 times more impact-resistant than standard acr.. |
|||
Tensile Creep Modulus, 1000 hours | 1200 - 1600 MPa | 174000 - 232000 psi | Average value: 1400 MPa Grade Count:4 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |