Polymer Property : Tensile Creep Modulus, 1000 hours = 1000 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
Arkema Group Oroglas® DRM Acrylic, Extrusion Grade  (discontinued **)
OROGLAS DRM is an extrusion grade that offers the typical properties of high impact acrylic combined with matte surface finishing.OROGLAS DRM is recommended for extrusion of sheets for lighting, pr..
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
Arkema Group Oroglas® DRT Acrylic, Impact Grade  (discontinued **)
For extrusion and injection molding applications. OROGLAS DRT combines good thermal resistance with an excellent impact resistance.Key features : impact resistance: up to 10 times more impact-resis..
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade  (discontinued **)
OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :..
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
ISO 899-1
Lanxess Pocan® S 1517 000000 PBT
PBT, non-reinforced, injection molding, extrusion, impact modified
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
ISO 899
BASF Ultraform N 2640 Z4 UNC Q600 POM
Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade.
Tensile Creep Modulus, 1000 hours 1000 MPa

@Strain <=0.500 %
145000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultraform® N2320 0035 LEV POM
Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
ISO 899-1
BASF Ultraform® S2320 0035 LEV POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
ISO 899-1
BASF Ultraform® S2320 0035 POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
ISO 899-1
BASF Ultraform® W2320 U035 LEV POM
Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
Tensile Creep Modulus, 1000 hours 1000 MPa

@Strain <=0.500 %
145000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultraform® N2320 0035 POM
Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF
Tensile Creep Modulus, 1000 hours 1000 MPa

@Strain <=0.500 %
145000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultraform® W2320 0035 POM
Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF
Tensile Creep Modulus, 1000 hours 1000 - 1800 MPa
145000 - 261000 psi
Average value: 1580 MPa Grade Count:4
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
Arkema Group Oroglas® SG 10 Acrylic, Gamma Radiation Resistant  (discontinued **)
OROGLAS SG 10 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no advers..
Tensile Creep Modulus, 1000 hours 1000 MPa
145000 psi
ISO 899-1
BASF Ultraform® W2320 0035 LEV POM
Description: Is a POM, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF