Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 2500 - 10000 MPa
363000 - 1.45e+6 psi
Average value: 7610 MPa Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Tensile Creep Modulus, 1000 hours 8500 - 10000 MPa
1.23e+6 - 1.45e+6 psi
Average value: 9130 MPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..