Polymer Property : Tensile Creep Modulus, 1000 hours = 1.09e+6 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 7500 - 12000 MPa
1.09e+6 - 1.74e+6 psi
Average value: 9170 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Tensile Creep Modulus, 1000 hours 7500 MPa

@Temperature 23.0 °C
1.09e+6 psi

@Temperature 73.4 °F
50%RH; ISO 899
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h..
Tensile Creep Modulus, 1000 hours 7500 - 15800 MPa
1.09e+6 - 2.29e+6 psi
Average value: 11800 MPa Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Tensile Creep Modulus, 1000 hours 7500 MPa

@Strain <=0.500 %
1.09e+6 psi

@Strain <=0.500 %
ISO 899-1
Styrolution Luran® 378 P G7 35% Glass Filled SAN
Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Tensile Creep Modulus, 1000 hours 7500 MPa
1.09e+6 psi
ISO 899-1
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 7500 MPa

@Time 3.60e+6 sec
1.09e+6 psi

@Time 1000 hour
50%RH; ISO 899-1
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
Tensile Creep Modulus, 1000 hours 7500 MPa
1.09e+6 psi
ISO 899-1
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 7500 MPa

@Strain <=0.500 %
1.09e+6 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..
Tensile Creep Modulus, 1000 hours 7500 MPa

@Strain <=0.500 %
1.09e+6 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Tensile Creep Modulus, 1000 hours 7500 MPa
1.09e+6 psi
ISO 899
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Tensile Creep Modulus, 1000 hours 7500 MPa

@Strain <=0.500 %
1.09e+6 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT
Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, ..