Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 7500 - 15800 MPa
1.09e+6 - 2.29e+6 psi
Average value: 11800 MPa Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..