Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin Film Properties. Features: Free flowing granules, toughness and strength, ease of extrusion.Applications: Blending, concentrates.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® LF-0718-A LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, bags-on-roll, garment film.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips Dynex™ D605A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ISO 5527 |
Total Finathene® LL 6010 FE 18P LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Huntsman PE5030 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Huntsman PE5032 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, excellent heat sealability, good adhesion, low smoking, no edge weave, and excellent printability.Applications: Extrusion: c.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-B Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Trash bags, liners, general packaging.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Industrial liners, heavy duty bags.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
ExxonMobil Escorene® LD-144 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin Film Properties. Features: Toughness and strength, thin films.Applications: Trash bags, garment film, bags-on-roll.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-F Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Stretch wrap, blend resin, industrial packaging.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, general purpose packaging, garment film.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Metabolix M-veraâ„¢ B5008 Film Grade Compostable Bioplastic B5008 is a compostable film product with 30% biobased carbon content that is ideal for compost bags and can liners used for organic waste diversion and for shopping and retail bags.Features:Meets re.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | Film value |
Dow DOWLEX™ 2267A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2267A Polyethylene resin is a high performance blown film polymer offering superior load retention and toughness for a variety of stretch film packaging applications. This material complies.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | 1%, Flexural; ASTM D882 |
Braskem Flexus® 7200 LLDPE Cast Film Extrusion Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | 1%; ASTM D882 |
Braskem LHB 118/21 AF LLDPE Blown Film Extrusion Polyethylene Description: LHB118/21 AF is a LLDPE copolymer produced by Braskem. It is a ready-to-use product since it contains 10% LDPE. Its additive package was optimized to avoid blocking, even at low thickne.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Sclair® 11N1 PE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe.. |
|||
Secant Modulus, MD | 0.180 GPa | 26.1 ksi | 1%; ASTM D882 |
Braskem LL 118 LLDPE Blown Film Extrusion Polyethylene Description: LL118 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for blown film extrusion in blends with polyethylenes. Films obtained with t.. |