Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en.. |
|||
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | ASTM D882 |
Eastman 5265 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Good optical properties, Superior impact strength, Low coefficient of friction, Good processability, High Slip, High Ant.. |
|||
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | ASTM D882 |
Eastman 5267 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Excellent impact strength, Good optical properties, Good processability, High antiblock, No slipApplications:Laminations.. |
|||
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | ASTM D882 |
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par.. |
|||
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | ASTM D882 |
Eastman 5282 LDPE 8% EVA Copolymer, High Clarity, High Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, Low Slip, High Antiblock, Good Bubble Stability at High Draw Down Speeds.. |
|||
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | ASTM D882 |
Eastman 5284 LDPE 8% EVA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, No Slip, High Antiblock, High Coefficient of FrictionApplications:Ice Ba.. |
|||
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light.. |
|||
Secant Modulus, MD | 0.110 GPa | 16.0 ksi | ASTM D882 |
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin.. |