Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , LLDPE
Manufacturer Petroquimica Triunfo
Trade Name Trilene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and ensuring the production of films with uniform thickness and good balance between the mechanical and optical properties. The additive package gives it thermal stability, low blocking, and adequate slip performance, which are indispensable to allow high productivity on the extrusion, printing, and finishing lines. The resin should be processed in extruders that are designed or adapted for LLDPE. The components that form the product Trilene® TS 8057 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.Applications: Technical laminated films designed for packaging of various products such as coffee, crackers, etc. Technical films for automatic or semi-automatic packaging of solid and liquids products and frozen foods. Bags and packaging for thin films in general. Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 50.0 microns
1.97 mil
Melt Index of Compound 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 870 %
870 %
ASTM D882
Film Elongation at Break, TD 995 %
995 %
ASTM D882
Secant Modulus, MD 0.110 GPa
16.0 ksi
5%; ASTM D882
Secant Modulus, TD 0.115 GPa
16.7 ksi
5%; ASTM D882
Coefficient of Friction, Dynamic 0.18
0.18
ASTM D1894
Elmendorf Tear Strength, MD 6.50 g/micron
165 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 18.7 g/micron
475 g/mil
ASTM D1922
Dart Drop Test 190 g
0.419 lb
(method A); ASTM D1709
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003
Gloss 106 %
106 %
@ 60° Gardner; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 180 - 190 °C
356 - 374 °F
Plasticizing Zone
190 - 200 °C
374 - 392 °F
Mixture Zone
Feed Temperature 180 - 190 °C
356 - 374 °F
Adapter Temperature 190 - 205 °C
374 - 401 °F
Die Cooling Temperature 200 - 215 °C
392 - 419 °F
Die Opening 0.180 - 0.250 cm
0.0709 - 0.0984 in
Blow-up Ratio (BUR) 3.0
3.0
Recommended
Descriptive Properties Value Comments
Proportion LLDPE % 75