Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.276 MPa | 40.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/16 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.276 MPa | 40.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-49 - 1/4 - 2.1 Woven Kevlar Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-49 is manufactured using KEVLAR® 49 fabric. A thermosetting adhesive is used for the node bonds and a 350°F cure modified epoxy resin i.. |
|||
Shear Strength | >= 0.276 MPa | >= 40.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRP/F35 - 2.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Shear Strength | >= 0.276 MPa | >= 40.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRH-10 - 1/4 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | >= 0.276 MPa | >= 40.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | >= 0.276 MPa | >= 40.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRH-10 - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.276 MPa | 40.0 psi | 2024 T3 Aluminum, 180°, after 48 hrs at 23°C |
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives 3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M |
|||
Shear Strength | 0.276 - 0.414 MPa | 40.0 - 60.0 psi | Overlap, Neoprene Rubber/Steel |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 0.276 - 0.414 MPa | 40.0 - 60.0 psi | Overlap, Neoprene Rubber/Steel |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |