Mechanical Properties Metric English Comments
Shear Strength 10.3 - 17.2 MPa
1500 - 2500 psi
ND Industries 533 Retaining Compound
High strength sealing applications for non migration material
Shear Strength 11.0 - 17.2 MPa
1600 - 2500 psi
ND Industries High Temperature SuperGlue 362
Medium viscosity with thermal cycling resistance
Shear Strength 7.58 - 17.2 MPa
1100 - 2500 psi
Average value: 13.2 MPa Grade Count:3
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..
Shear Strength 13.8 - 17.2 MPa
2000 - 2500 psi
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati..
Shear Strength 16.5 - 17.2 MPa
2400 - 2500 psi
CRS Overlap
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e..