Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 7.58 - 17.2 MPa | 1100 - 2500 psi | Average value: 13.2 MPa Grade Count:3 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Shear Strength | >= 7.58 MPa | >= 1100 psi | Al/Al, tensile |
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation .. |
|||
Shear Strength | >= 7.58 MPa | >= 1100 psi | Al/Al, bond |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Tensile lap, Polycarbonate/Polycarbonate |
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Long Beam Shear, W Direction |
Hexcel® HexWeb® HDC-660 - 3/16 - 17.5 (R2) Heavy Density Core Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with eit.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Lap |
Epoxy Technology EPO-TEK® 301-1 Optical Grade Epoxy Material Description: A two component, room temperature curing, optical grade epoxy, designed for optics, medical, and opto-electronic packaging of semiconductor devices, components, and electronics.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | CRS Overlap, White Gas @ RT |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, HDPE, Substrate Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Polycarbonate, Adhesive Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, 304 Stainless Steel (1/32" thick), Cohesive Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Control, Substrate Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, HDPE, Substrate Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Control, Substrate Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Control, Substrate Failure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Acrylic, Substrate Failure |
3M Scotch-Weld™ DP8805NS Low Odor Acrylic Adhesives 3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and .. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Cold Rolled Steel-MEK/abrade/MEK |
3M Scotch-Weld™ DP100 FR Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ DP-5106 Control Joint Sealant 3M™ Scotch-Weld™ Control Joint Sealant DP-5106 is a self-leveling, gray, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in duo-pak cartridges. With the squeeze of t.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, HDPE, Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, PP, Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Control, Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, HCl, Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa @Temperature 23.0 °C |
1100 psi @Temperature 73.4 °F |
Overlap, HDPE, Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa @Temperature 23.0 °C |
1100 psi @Temperature 73.4 °F |
Overlap, Green FRP, Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Acrylic, Substrate Failure |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 7.58 MPa @Temperature 66.0 °C |
1100 psi @Temperature 151 °F |
Overlap, Pine, Adhesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Acrylic/Acrylic; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 7.58 MPa | 1100 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Phenolic |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |