Polymer Property : Shear Strength = 1600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 11.0 - 17.2 MPa
1600 - 2500 psi
ND Industries High Temperature SuperGlue 362
Medium viscosity with thermal cycling resistance
Shear Strength 11.0 MPa

@Temperature 65.6 °C,
Time 7200 sec
1600 psi

@Temperature 150 °F,
Time 2.00 hour
Lap
Parker Chomerics CHO-BOND 360-20 Conductive Epoxy
Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E..
Shear Strength 11.0 MPa
1600 psi
Cured 30 minutes at 150°C, Al/Al
Resin Technology Group TIGA 908 Gold Bonder - Low Stress Silver Conductive
100 parts resin to 6 parts hardener.TIGA 908 is a low stress, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications which require bonding to gol..
Shear Strength 11.0 - 164.095 MPa

@Temperature -55.0 - 177 °C
1600 - 23800.0 psi

@Temperature -67.0 - 351 °F
Average value: 58.8 MPa Grade Count:26
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Shear Strength 11.0 MPa
1600 psi
Shear Bond Holding Strength
Indium Corp. Indalloy® 3 In-Ag Solder Alloy
Has nearly the wettability and low temperature malleability of Indium. Solders silver, fired glass, and ceramics. Large plastic range.Information provided by the manufacturer, Indium Corporation.
Shear Strength 11.0 - 13.8 MPa
1600 - 2000 psi
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Shear Strength 11.0 MPa
1600 psi
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech..
Shear Strength 11.0 MPa
1600 psi
Bond, Al to Al, RT cure
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant
Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated..
Shear Strength 11.0 MPa
1600 psi
Overlap, Fiberglass
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Shear Strength 11.0 MPa

@Temperature -29.0 °C
1600 psi

@Temperature -20.2 °F
Overlap, Adhesion Failure
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 11.0 MPa
1600 psi
Overlap, Wood (Fir) (dry wipe)-Substrate Failure; ASTM D1002
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Shear Strength 11.0 MPa
1600 psi
Overlap, FR-4/FR-4 tested after 90°C/2 wks/90% RH
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..