Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 530 g | 530 g | ASTM D 1992 |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |
|||
Elmendorf Tear Strength TD | 530 g | 530 g | ASTM D1922 |
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin Product Description: Exact 3040 is an ethylene-based hexane copolymer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monolayer and coextrusion cast fi.. |
|||
Elmendorf Tear Strength TD | 530 g | 530 g | ASTM D1922 |
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin.. |
|||
Elmendorf Tear Strength TD | 530 g | 530 g | ASTM D1922 |
Huntsman Rexell® V3401 Blown Film Extrusion LLDPE
(discontinued **) Ultra linear low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability, toughness, and optics with good sealing properties.Applications: Sealing layer in coextrude.. |