Total HL 428 HDPE film resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Total Atofina
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HL 428 HDPE film resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ASTM D 792
Water Vapor Transmission 7.76 g/m²/day
0.500 g/100 in²/day
E 96/66
Thickness 25.4 microns
1.00 mil
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
High Load Melt Index 20 g/10 min

@Load 21.6 kg
20 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD >= 25.5 MPa
>= 3700 psi
ASTM D 882 A
Film Elongation at Break, MD 600 %
600 %
ASTM D 882 A
Film Elongation at Break, TD 700 %
700 %
ASTM D 882 A
Elmendorf Tear Strength MD 28 g
28 g
ASTM D 1922
Elmendorf Tear Strength TD 530 g
530 g
ASTM D 1992
Dart Drop Test 100 g
0.221 lb
ASTM D 1709 A
Film Tensile Strength at Break, MD >= 54.5 MPa
>= 7900 psi
ASTM D 882A
Film Tensile Strength at Break, TD >= 39.3 MPa
>= 5700 psi
ASTM D 882 A
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ASTM D3417