Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 38.0 - 47.0 MPa | 5510 - 6820 psi | Average value: 42.5 MPa Grade Count:3 |
Overview of materials for Nylon 11, Powder This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | 38.0 - 47.0 MPa | 5510 - 6820 psi | |
Arkema Group Rilsan® Fine Powders Grey 49 Polyamide 11 Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p.. |
|||
Tensile Strength, Ultimate | 38.0 - 47.0 MPa | 5510 - 6820 psi | |
Arkema Group Rilsan® Fine Powders Natural Polyamide 11 Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p.. |
|||
Tensile Strength, Ultimate | 38.0 - 47.0 MPa | 5510 - 6820 psi | |
Arkema Group Rilsan® Fine Powders Polyamide 11 Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p.. |