Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® Fine Powders Grey 49 Polyamide 11

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Powder
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® Fine Powders Grey 49 Polyamide 11.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum products.Typical Applications:Shopping carts Dishwasher baskets Hand mixers File rods Wire shelvesInformation provided by Arkema Group
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.0 - 47.0 MPa
5510 - 6820 psi
Taber Abrasion, mg/1000 Cycles 17
17
CS 17 wheel, 1 kg load
Thermal Properties Metric English Comments
Heat of Fusion 83.7 J/g
36.0 BTU/lb
CTE, linear 150 µm/m-°C

@Temperature 20.0 °C
83.3 µin/in-°F

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 3.50e+14 ohm-cm

@Temperature 20.0 °C
3.50e+14 ohm-cm

@Temperature 68.0 °F
65% RH at 500 V; ASTM D257
Surface Resistance 2.40e+14 ohm

@Temperature 20.0 °C
2.40e+14 ohm

@Temperature 68.0 °F
65% RH at 500 V; ASTM D257
Dielectric Constant 3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
3.9

@Frequency 100 Hz
3.9

@Frequency 100 Hz
Dielectric Strength 9.00 kV/mm

@Thickness 0.400 mm
229 kV/in

@Thickness 0.0157 in
thick
Users viewing this material also viewed the following: