3M Jet-Weld™ TE-015 Adhesive

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer 3M
Trade Name Jet-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Jet-Weld™ TE-015 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly.Extrudable. Very fast set time for bonding wood and selected plasticsInformation provided by 3M
Physical Properties Metric English Comments
Viscosity 7000 cP
7000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Ultimate 27.2 MPa
3950 psi
Elongation at Break 750 %
750 %
Modulus of Elasticity 0.0172 GPa
2.50 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F