Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate >= 240 MPa
>= 34800 psi
Kobe Steel KS40 Commercially Pure Titanium, ASTM Gr. 1, Annealed
Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel
Tensile Strength, Ultimate >= 240 MPa
>= 34800 psi
Kobe Steel KS40PDA Titanium alloy with low alloying elements, ASTM Gr. 11, Annealed
Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by ..
Tensile Strength, Ultimate >= 240 MPa
>= 34800 psi
Kobe Steel KS40S Commercially Pure Titanium, ASTM Gr. 1, Annealed
Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; A (TB00) Temper (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate >= 240 MPa
>= 34800 psi
MetalTek MTEK 65 UNS C90700 Gear Bronze
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C90700; Cast Grade C90..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; A (TB00) Temper (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 MPa
34800 psi
Zoltek Pyron® Continuous Tow Oxidized Pan Fiber
Oxidized Pan FiberApplications include: Yarn Stretch Breaking, Pulp Milling, Staple Fiber Chop for Nonwovens or Yarn Spinning
Tensile Strength, Ultimate 240 MPa
34800 psi
dry; ISO 527-1/-2
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
Tensile Strength, Ultimate 240 MPa
34800 psi
dry; ISO 527-1/-2
DSM Stanyl® TW200B6 PA46-CF30
30% Carbon Reinforced, Heat Stabilized, Lubricated
Tensile Strength, Ultimate 240 MPa
34800 psi
dry; ISO 527-1/-2
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
Tensile Strength, Ultimate 240 MPa

@Temperature 200 °C
34800 psi

@Temperature 392 °F
Typical, after 10,000 hours
Aleris Weldural Aluminum Alloy, 100 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Tensile Strength, Ultimate 240 MPa
34800 psi
dry; ISO 527-1/-2
DSM Novamid® MC112LG55 C10 PA6-GF55
55% Glass Reinforced
Tensile Strength, Ultimate 240 MPa
34800 psi
ISO 527
LATI LARAMID G/50 50% Glass Filled Polyphthalamide (PPA) Based Compound  (Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Tube; A (TB00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..