Zoltek Pyron® Continuous Tow Oxidized Pan Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Pyron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Pyron® Continuous Tow Oxidized Pan Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxidized Pan FiberApplications include: Yarn Stretch Breaking, Pulp Milling, Staple Fiber Chop for Nonwovens or Yarn Spinning
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
1.40 g/cc
0.0506 lb/in³
Fineness 1.7
1.7
Fineness, dTex
2.2
2.2
Fineness, dTex
5.0
5.0
Fineness, dTex
Filament Diameter 12.5 µm
12.5 µm
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 240 MPa
34800 psi
Component Elements Properties Metric English Comments
Carbon, C 62 %
62 %
Loss on Ignition(%) >= 40 %
>= 40 %
>= 50 %
>= 50 %
Descriptive Properties Value Comments
Filament Count 300000
Format, crimp level/inch Uncrimped