Polymer Property : Tensile Strength, Ultimate = 294 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 - 294 MPa
7250 - 42600 psi
Average value: 182 MPa Grade Count:253
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Tensile Strength, Ultimate 138 - 294 MPa
20000 - 42600 psi
Average value: 208 MPa Grade Count:17
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..