Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.90 - 26.8 MPa | 276 - 3890 psi | Average value: 12.7 MPa Grade Count:70 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Ultimate | 1.90 MPa | 276 psi | ASTM D638 |
ExxonMobil Escorene® LD-752 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Tensile Strength, Ultimate | 1.90 MPa | 276 psi | ASTM D638 |
ExxonMobil Escorene® UL-7720 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Tensile Strength, Ultimate | 1.90 MPa | 276 psi | |
Indium Corp. Indalloy® 4 Pure Indium Solder Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni.. |
|||
Tensile Strength, Ultimate | 1.90 MPa | 276 psi | ASTM D412 |
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant High strength, two-part structural glazing system. Cure Method: Condensation. Tack-free time 3 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of .. |
|||
Tensile Strength, Ultimate | 1.90 - 5.70 MPa | 276 - 827 psi | Average value: 3.24 MPa Grade Count:7 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |