Momentive Performance Materials Ultraglaze® 4400 Construction Sealant

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Construction Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name Ultraglaze®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Ultraglaze® 4400 Construction Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength, two-part structural glazing system. Cure Method: Condensation. Tack-free time 3 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ASTM D2240
Tensile Strength, Ultimate 1.90 MPa
276 psi
ASTM D412
Tensile Strength, Yield 0.590 MPa
85.6 psi
at 50% Extension (0.5 x 0.38 x 2 in bead)
Elongation at Break 200 %
200 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 88.0 °C
190 °F
Elasticity is retained to this temperature.
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Elasticity is retained to this temperature.
Processing Properties Metric English Comments
Processing Temperature 27.0 °C
80.6 °F
Cure time to 0.38 in. is 5-7 days