Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 63.0 - 165 MPa | 9140 - 24000 psi | Average value: 103 MPa Grade Count:31 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 45.0 - 165 MPa | 6530 - 24000 psi | Average value: 81.1 MPa Grade Count:32 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Tensile Strength, Ultimate | 103 - 166 MPa | 15000 - 24000 psi | Average value: 143 MPa Grade Count:30 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Tensile Strength, Ultimate | 114 - 165 MPa | 16500 - 24000 psi | Average value: 137 MPa Grade Count:10 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Ultimate | 70.0 - 165 MPa | 10200 - 24000 psi | Average value: 123 MPa Grade Count:38 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |