Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 17.0 - 216 MPa @Temperature -40.0 - 250 °C |
2470 - 31300 psi @Temperature -40.0 - 482 °F |
Average value: 86.6 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 17.0 - 216 MPa @Thickness 1.60 - 3.17 mm |
2470 - 31300 psi @Thickness 0.0630 - 0.125 in |
Average value: 86.6 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |