ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of similar materials.Applications: Compound viscosity modifier; High flow applications.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
Exxon Method
Apparent Bulk Density 0.577 g/cc
0.0208 lb/in³
ASTM D1895 (B)
Viscosity 9300 cP

@Temperature 190 °C
9300 cP

@Temperature 374 °F
melt viscosity; ASTM D-3236
Melt Flow 800 g/10 min
800 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 70.0 °C
158 °F
Exxon Method
Vicat Softening Point 87.0 °C
189 °F
Softening Point, R&B; ASTM E-28