Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Carbon Fiber Filled
Manufacturer Techmer ES
Trade Name Electrafil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Water Absorption 1.0 %
1.0 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 131 MPa
19000 psi
ASTM D638
Tensile Modulus 7.93 GPa
1150 ksi
ASTM D638
Flexural Yield Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 7.24 GPa
1050 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D4496