Technetics Group Amicon™ PEEK 30% Carbon  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Technetics Group Amicon™ PEEK 30% Carbon  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Technetics Group (formerly Plastomer Technologies)
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Water Absorption 0.060 %
0.060 %
24 hours; ASTM D570 (2)
Water Absorption at Saturation 0.30 %
0.30 %
ASTM D570 (2)
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 131 MPa
19000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Modulus of Elasticity 7.58 GPa
1100 ksi
ASTM D638
Compressive Strength 200 MPa
29000 psi
ASTM D695
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256 type "A"
Coefficient of Friction 0.20
0.20
ASTM PTM 55007
K (wear) Factor 302 x 10-8 mm³/N-M
150 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
4:1 safety factor
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 100 °C
10.0 µin/in-°F

@Temperature 212 °F
ASTM E-831 (TMA)
Maximum Service Temperature, Air 250 °C
482 °F
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
ASTM UL-94
Electrical Properties Metric English Comments
Dielectric Strength 1.26 kV/mm
32.0 kV/in
ASTM D149