Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 17.0 - 148 MPa | 2470 - 21500 psi | Average value: 70.8 MPa Grade Count:72 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |