Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 35.0 - 93.2 MPa | 5080 - 13500 psi | Average value: 67.7 MPa Grade Count:49 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Tensile Strength, Ultimate | 5.50 - 93.1 MPa | 798 - 13500 psi | Average value: 61.8 MPa Grade Count:22 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Tensile Strength, Ultimate | 50.0 - 93.0 MPa | 7250 - 13500 psi | Average value: 70.0 MPa Grade Count:17 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Tensile Strength, Ultimate | 46.1 - 93.1 MPa | 6690 - 13500 psi | Average value: 64.5 MPa Grade Count:208 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |