Polymer Property : Tensile Strength, Ultimate = 798 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
ASTM D638
Multibase Multi-Flex® TPE A 6821 BLK
This product is based on Kraton G and PP suitable for automotive applications and meets GM, Ford, and Chrysler specifications. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 5.50 MPa
798 psi
ASTM D412
Multibase Multi-Flex® TPE A 6821 C BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 5.50 MPa
798 psi
ASTM D638
Multibase Multi-Flex® TPE A 6821 NAT
This product is based on Kraton G and PP. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 5.50 MPa
798 psi
ASTM D638
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 84 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Tensile Strength, Ultimate 5.50 - 76.0 MPa
798 - 11000 psi
Average value: 13.1 MPa Grade Count:17
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 5.50 - 93.1 MPa
798 - 13500 psi
Average value: 61.8 MPa Grade Count:22
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Tensile Strength, Ultimate 5.50 MPa
798 psi
ASTM D412
Momentive Performance Materials UltraSpan® Weatherstrip
Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Tensile Strength, Ultimate 5.50 MPa
798 psi
Indium Corp. Indalloy® 290 In-Ag Solder Alloy
Indium with silver added to improve strength. Has the wettability and low-temperature malleability of indium. Particularly useful for cryogenic applications.Information provided by the manufacturer,..
Tensile Strength, Ultimate 5.50 MPa

@Temperature 49.0 °C
798 psi

@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Tensile Strength, Ultimate 5.50 MPa

@Temperature 49.0 °C
798 psi

@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
Arlon 0.010" (0.254 mm) Flexible Heater Silicone with Fiberglass Substrate (49586R010)
Cured silicone rubber with a minimum thickness of 0.0015 in. (0.038 mm)/ 0.0055 in. (0.14 mm) Prime Coated 1681 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.003 in. (0.08 mm); 0...
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51571R015)
Cured silicone rubber with a minimum thickness of 0.0035 in. (0.08 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.1 mm); 0.003..
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51576R015)
Cured silicone rubber with a minimum thickness of 0.002 in. (0.05 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.005 in. (0.1 mm); 0.003 i..
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579A028)
0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over..
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579GA028)
0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over..
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579R028)
0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over..
Tensile Strength, Ultimate >= 5.50 MPa
>= 798 psi
Arlon 0.008" (0.2032 mm) Flexible Heater Silicone with Fiberglass Substrate (49580R010)
Uncured silicone rubber with a minimum thickness of 0.0045 in. (0.11 mm) on 0.0055 in. (0.14 mm) Prime Coated 1681 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.010 in..