Material Notes:
SUPERPLAST® Stainless is a specially designed steel for plastic mould bases providing improved performances compared to standard grades such as 1.2085. SUPERPLAST® Stainless offers improved machinability, improved consistency and weldability, and increased thermal conductivity. Moreover, thanks to its low Carbon and 13% Chromium content, SUPERPLAST® Stainless ensures a good corrosion resistance (atmospheric as well as from acidic polymers). SUPERPLAST® Stainless offers significantly improved machinability (tool life and chip removal) when compared to 1.2085 commonly used for this application. The steel provides also an improved dimensional stability after machining, thanks to its balanced chemical composition and special heat treatment. Nevertheless, SUPERPLAST® is not recommended for texturing and polishing.
Mechanical Properties Metric English Comments
Hardness, Brinell 322
322
40 mm from surface
322
322
60 mm from surface
323
323
20 mm from surface
324
324
0 mm from surface
324
324
80 mm from surface
324
324
105 mm from surface
325
325
108 mm from surface
325
325
100 mm from surface
Tensile Strength, Ultimate 1060 MPa
154000 psi
Tensile Strength, Yield 870 MPa
126000 psi
Elongation at Break >= 11 %
>= 11 %
Thermal Properties Metric English Comments
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.040 %
<= 0.040 %
Chromium, Cr 13 %
13 %
Iron, Fe >= 86.72 %
>= 86.72 %
Silicon, Si 0.10 %
0.10 %
Sulfur, S <= 0.14 %
<= 0.14 %