Misumi G-STAR Martensite Free-cutting Stainless Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel
Manufacturer Misumi
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Misumi G-STAR Martensite Free-cutting Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation.
Physical Properties Metric English Comments
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 33.0 - 37.0
33.0 - 37.0
Tensile Strength, Ultimate 1060 MPa
154000 psi
Tensile Strength, Yield 855 MPa
124000 psi
Elongation at Break 16.0 %
16.0 %
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 - 100 °C
5.72 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 25.1 W/m-K
174 BTU-in/hr-ft²-°F
Users viewing this material also viewed the following: