Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 483 MPa @Diameter 47.63 - 73.03 mm |
>= 70000 psi @Diameter 1.875 - 2.875 in |
ASTM E-8 |
H.C. Starck Pure Molybdenum AB, Arc-Cast Bar Arc-Cast BarDescription of Product: This specification covers carbon-deoxidized molybdenum wrought bar produced from ingots consolidated by the H.C. Stark consumable electrode vacuum-arc-casting pr.. |
|||
Tensile Strength | >= 483 MPa @Diameter 47.63 - 73.03 mm |
>= 70000 psi @Diameter 1.875 - 2.875 in |
ASTM E-8 |
H.C. Starck Pure Molybdenum ABL, Arc-Cast, Low Carbon Bar Description of Product: This specification covers carbon-deoxidized, low-carbon molybdenum wrought bar produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting p.. |
|||
Tensile Strength | 483 - 621 MPa @Thickness >=25.4 mm |
70000 - 90000 psi @Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu.. |