Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 483 - 621 MPa @Thickness >=25.4 mm |
70000 - 90000 psi @Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu.. |